Cracking paste 咨询谢燕红 12 |
State | Paste |
Packing | 25KG/drum for white, 20KG/drum for clear |
Storage | 6 months in cool place |
Suitable for knitting |
Features | 1. High fastness2. High softness3. SGS detecting passed, no PVC, no heavy metal, no NPEOs. |
Mix proportion | Light: White cracking paste 70-100% + Clear cracking paste 0-30% + pigment ?% + fixing agent 2%Deep: White cracking paste 20-30% + Clear cracking paste 70-80% + pigment ?% + fixing agent 2% |
Printing process | 1. Printing with clear cracking paste ( for underbase) for 1-2 times2. Mixing with white cracking paste, clear cracking paste, pigment, fixing agent and stirring them evenly.3. Printing again for 2-3 times (3-4 scrapes per time).4. Drying the paste surface with cold air, it will be cracked by itself after it’s dry.5. Hot pressing the printing for about 5 seconds with 150℃ to make it better adhesion.6. Finish. |
Attentions | 1. Thick screen is suggested for the best effect (print for 1 time only). If with thin screen, please printing for 2-3 times, and blow the paste surface with cold air to dry it fast and re-printing before it’s cracked.2. Please take the fabric up after i pletely cracked, otherwise it’s won’t be cracked naturally.3. More clear and thinner the paste is , thinner the crack is.4. Th n not be exceeded in 12%, otherwise it'll be easily faded. |
品名 | 耐水洗龟裂浆 咨询谢燕红 12 |
外观 | 糊状 |
包装 | 白胶浆25KG/桶,透明浆20KG/桶,打底透明浆20KG/桶 |
贮存期 | 常温下6个月 |
应用 | 针织布 |
卖点 | 1. 高牢度耐水洗2. 手感柔软3. 符合美国ASTM对邻苯二甲酸脂和欧盟EN71 Part 3对重金属含量的要求 |
调配比例 | 印浅色:龟裂白胶浆70-100% +龟裂透明浆0-30% + 色浆?% + 固化剂2%印深色:龟裂白胶浆20-30% + 龟裂透明浆70-80% + 色浆?% + 固化剂2% |
工艺流程 | 1. 丝网选用80-100目,用丝印硬方刀75度刮印,先用龟裂打底透明浆打底印1-2次, 第一板用力刮4-6刀2. 将龟裂白胶浆,透明浆,色浆,固化剂搅拌均匀印2-3次(每次刮3-4刀)3. 自燃干燥爆裂4. 起布 |
注意事项 | 1. 印裂纹浆必须先打底才能保证水洗牢度2. 若胶浆印前太稠可加水,切勿加固浆以免影响裂纹效果3. 建议晒厚网印龟裂浆,一次印够色为最佳.若用薄网印刷,请用冷风吹浆层的表面,在浆层还没有裂开之前返印.(裂纹的大小与多少可以在龟裂白和龟裂透明的互配比例和印出来的浆层厚薄控制,龟裂透明比例越多和印出来的浆层越薄它的裂纹就越细,反之它的裂纹越粗 咨询谢燕红 12 |