20mm | Q345D-Z35 | 切边 | 10500 | 2500 | 1 | 4.121 |
20mm | Q345D-Z35 | 切边 | 10500 | 2500 | 1 | 4.121 |
20mm | Q345D-Z35 | 切边 | 10500 | 2500 | 1 | 4.121 |
20mm | Q345D-Z35 | 切边 | 10600 | 2500 | 1 | 4.161 |
20mm | Q345D-Z35 | 切边 | 10500 | 2500 | 1 | 4.121 |
20mm | Q345D-Z35 | 切边 | 10600 | 2500 | 1 | 4.161 |
20mm | Q345D-Z35 | 切边 | 10600 | 2500 | 1 | 4.161 |
调质钢化学成分
牌号 | 质量等级 | 化学成分 |
C | Si | Mn | Nba | Va | Tia | Alsa,b | Cr | Ni | Cu | Mo | N |
不大于 |
Q500q | DEF | 0.11 | 0.55 | 0.80~1.70 | 0.050~0.060 | 0.010~0.080 | 0.006~0.030 | 0.010~0.045 | ≤0.80 | ≤0.70 | ≤0.30 | ≤0.30 | 0.0080 |
Q550q | 0.12 |
Q620q | 0.14 | 0.005~0.090 | 0.40~0.80 | 0.25~1.00 | 0.15~0.55 | 0.20~0.50 |
Q690q | 0.15 | 0.40~1.00 | 0.25~1.20 | 0.20~0.60 |
注:可添加B元素0.0005%~0.0030% |
a 钢中AL、Nb、V、Ti可单独或组合加入,单独加入时,应符合表中规定;组合加入时,应至少保证一种合金元素含量达到表中下线规定,且Nb+V+Ti≤0.22%c 当采用全铝(Alt)含量计算时,全铝含量应为0.015%~0.050%。 |
汽车车轮用热轧钢带:AG330CL/AG380CL/AG400CL/AG420CL/AG490CL
汽车大梁用高强度热轧卷板:AG 590L/AG640L/AG700L/AG800L
汽车机械搅拌罐用热轧卷板:AG520JJ/AG620JJ 汽车车厢用热轧卷板:AG 600XT/AG500XT/AG600CXT
汽车挂车车厢用热轧卷板:AG600CXT/AG700XT
高强度汽车用热轧卷板 :AG700MC/AG700ZT
汽车大梁用热轧卷板 :QSTE340TM/QSTE380TM/QSTE420TM/QSTE460TM/QSTE500TM/QSTE550TM