项目 Item | 指标 Indexes |
N-1 | N-2a |
耐火度/Refractoriness (℃) | 1750 | 1730 |
2Kgf/cm2荷重软化开始温度 (℃) Refractoriness under load | ≥1400 | ≥1350 |
重烧线变化 % 1400℃,2h Permanent Linear Change | -0.4 | -0.3 |
显气孔率/Apparent Porosity % | ≤22 | ≤23 |
常温耐压强度/Cold crushing strength MPa | ≥35 | ≥32 |
热震稳定性次数/Thermal shock resistance |