详细说明
台州PA66美国杜邦70G35HSLRA4价格与物性表,上海PA66美国杜邦70G35HSLRA4报价,武汉PA66美国杜邦70G35HSLRA4批发价格
DuPont Zytel® nylon resin
杜邦Zytel® 尼龙树脂
Glass Reinforced Resins
玻璃纤维增强树脂
Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.
zytel®70G35HSLRA4 BK267是一个35%玻璃纤维增强,热稳定,抗水解聚酰胺66树脂注塑。它具有优异的流动特性。
Property | Test Method | Units | Value |
DAM | 50%RH |
IdentificationResin IdentificationPart Marking Code | ISO 1043ISO 11469 | | PA66-GF35>PA66-GF35 |
MechanicalStress at BreakStrain at BreakTensile ModulusNotched Charpy Impact StrengthUnnotched Charpy Impact Strength | ISO 527ISO 527ISO 527ISO 179/1eAISO 179/1eU | MPa(kpsi)%MPa(kpsi)2kJ/m2kJ/m | 210(30.5)311200(1600)1580 | 140(20.3)57800(1130)1895 |
ThermalDeflection Temperature1.80MPaMelting Temperature10℃/min | ISO 75-1/-2ISO 11357-1/-3 | ℃(℉)℃(℉) | 250(480)260(500) | |
OtherDensityMolding ShrinkageNormal, 2mmParallel, 2mm | ISO 1183ISO 294-4 | 3 3kg/m(g/cm )% | 1410(1.41)1.10.4 | |
PA66美国杜邦70G35HSLRA4
Property | Test Method | Units | Value |
DAM | 50%RH |
ProcessingMelt Temperature RangeMelt Temperature OptimumMold Temperature RangeMold Temperature OptimumDrying Time, Dehumidified DryerDrying TemperatureProcessing Moisture Content | | ℃(℉)℃(℉)℃(℉)℃(℉)h℃(℉)% | 285-305(545-580)295(565)70-120(160-250)100(210)2-480(175) |